MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celstran® PA66-GF40-02P11 Nylon 66, 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Material code according to ISO 1043-1: PA66

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 215 MPa5mm/min; ISO 527-2/1A
Elongation at Break 2.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 13000 MPa50mm/min; ISO 527-2/1A
Flexural Strength 200 MPaISO 178
Flexural Modulus 8100 MPaISO 178
 
Processing PropertiesOriginal ValueComments
Processing Temperature 90.0 - 120 °Ccavity
 300 - 315 °Chot runner
Feed Temperature 20.0 - 50.0 °C
Zone 1 280 - 285 °C
Zone 2 280 - 290 °C
Zone 3 290 - 300 °C
Zone 4 300 - 310 °C
Die Temperature 310 - 320 °C
Melt Temperature 310 - 320 °C
Drying Temperature 70.0 - 80.0 °C
Dry Time 2.00 - 4.00 hour
Moisture Content <= 0.15 %
Injection Pressure 120 - 150 MPa
Hold Pressure 50.0 - 80.0 MPa
Back Pressure <= 3.00 MPa
Screw Speed 25 rpm
@Diameter 75.0 mm
 35 rpm
@Diameter 55.0 mm
 50 rpm
@Diameter 40.0 mm
 
Descriptive Properties
Heat stabilized/stable to heatYes
Injection speedmedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Oxford Polymers PPS/66-505-40GF-BK PPS/PA66, 40% Glass Fiber Reinforced
Celanese Zytel® 70G30L NC010 PA66-GF30
Omnia Plastica PPS GF40 Polyphenylenesulphide
Domo TECHNYL® A 218 V40 Black 21 N PA 66 40% Glass Reinforced, Dry
Domo TECHNYL® A 218 V40 Black 21 N PA 66 40% Glass Reinforced, Conditioned

PHCQ164 / 178619

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.