MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tabriz HIPS 7350ESCR High impact polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: HIPS 7350 ESCR is a high impact polystyrene grade with improved stress cracking resistance compared to conventional high impact polystyrene. The excellent melt strength of this grade makes it particularly suited for deep-draw thermoforming. It offers good environmental stress crack resistance at low temperatures, rendering it suitable for frozen packaging, refrigerator liners and door paneling while retaining good mechanical properties. It is recommended for packaging applications such as oily food and dairy products. This grade has food contact approval. Applications: Sheet extrusion application, Refrigerator inner liner, Refrigerator door liner, Packaging applications for oily food and dairy products.

Information provided by Tabriz Petrochemical Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 20.0 MPaASTM D638
Tensile Strength, Yield 18.0 MPaASTM D638
Elongation at Break 50 %ASTM D638
Tensile Modulus 1600 MPaASTM D638
Izod Impact, Notched (ISO) 12.0 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 93.0 °C50°C/hr 1kg; ASTM D1525
 
Descriptive Properties
Styrene Residual Monomer<500 ppmCLG LABPSG004 (Atofina Test)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tabriz WT1235 High Impact Polystyrene
Americas Styrenics Styron® XL-8023VC High Impact Polystyrene
Americas Styrenics STYRON® EA6740 High Impact Polystyrene
Americas Styrenics Styron® 425 High Impact Polystyrene
Americas Styrenics STYRON® 404 High Impact Polystyrene

PTABRZ923 / 198234

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.