MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
General Plastics LAST-A-FOAM® R-3325 Submersible Foam Series
Categories: Other Engineering Material; Composite Core Material

Material Notes: Product Description: LAST-A-FOAM® R-3300 is an easy-to-machine, pressure-resistant foam that provides buoyancy for underwater depths tested to 2,400 feet, when coated. The closed-cell structure of this series is uniquely engineered to withstand penetration by water and resist hydrostatic pressure. LAST-A-FOAM® R-3300 submersible foam is optimal for shallow to mid-water subsea buoyancy systems, marine and underwater robotics applications.

Features & Benefits:

  • Provides buoyancy with depths to 1,200 feet uncoated and 2,400 feet coated
  • Excellent mechanical and insulation properties
  • Easy to machine, coat, and paint
  • Dimensionally stable
  • Resistant to hydrostatic pressure
  • High impact resistance
  • Biologically inert
  • Oil, grease, and solvent resistant
  • Cost-effective solution
  • Does not rot or decay
  • Performs in freshwater and saltwater
  • Compatible with many types of adhesives
Applications:
  • Underwater buoyancy
  • Underwater robotics (ROV/AUV)
  • Semi-submersible craft
  • Pipeline flotation
  • Subsea mooring buoyancy
  • Buoyancy for assembly components in weightlessness simulation pools
  • Underwater pumps for offshore drilling rigs
  • Core material for resin-transfer molding

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.400 g/ccASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 46cut foam surface; ASTM D2240
Tensile Strength 1479 psiPerpendicular to Rise; ASTM D1623
Flexural Strength 1875 psiRise Parallel to Specimen Width; ASTM D790 Method 1-A
 1876 psiRise Parallel to Beam Thick.; ASTM D790 Method 1-A
Flexural Modulus 53409 psiRise Parallel to Beam Thick.; ASTM D790 Method 1-A
 53981 psiRise Parallel to Specimen Width; ASTM D790 Method 1-A
Compressive Strength 952 psi
@Temperature 93.3 °C
Perpendicular to Rise; ASTM D1621
 973 psi
@Temperature 93.3 °C
Parallel to Rise; ASTM D1621
 1735 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 1748 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
Compressive Modulus 30511 psi
@Temperature 93.3 °C
Perpendicular to Rise; ASTM D1621
 31973 psi
@Temperature 93.3 °C
Parallel to Rise; ASTM D1621
 45704 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 48671 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
Shear Modulus 2.83 ksiRise Parallel to Specimen Thick.; ASTM C273
Shear Strength 0.327 ksiRise Parallel to Specimen Thick.; ASTM C273
 
Thermal PropertiesOriginal ValueComments
CTE, linear 32.0 µin/in-°F
@Temperature -45.6 - 93.3 °C
GP Method
Thermal Conductivity 0.415 BTU-in/hr-ft²-°FASTM C518
Glass Transition Temp, Tg 260 °FASTM E1824
 
Descriptive Properties
Closed Cell Content98%ASTM D6226
Depths Coated732 metersGP Method based on ASTM D570
Depths Uncoated366 metersGP Method based on ASTM D570
Hydrostatic TestingPass, <5% Wt Gainat 530 psi
Tumbling Friability (%)0.520 mins @ 60 rpm, ASTM C421

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-3703 Polyurethane Foam
Evonik ROHACELL® 50 WIND-F Polymethacrylimide Foam
Armacell ArmaFORM® GR70 PET foam core
J6 Polymers JFOAM™ HTC-12 Engineered Specialty Foam
General Plastics LAST-A-FOAM® WSF-1010 Foam

PGENR004 / 186790

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.