MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® TSS/2 FA PA666
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: Product description: Grilon TSS/2 FA is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/2 FA has the following important properties:
  • Excellent flow behavior
  • High toughness
  • Very good surface finish
  • Easy processing
Grilon TSS is used typically for various applications in the automotive, the electro and the sports & leisure field such as loudspeaker grids, interior casings, chair rollers, handles and levers. According to FDA (21 CFR 177.1500 and corresponding paragraphs covering the additives) GRILON TSS/2 FA is also approved for the direct contact with non-alcoholic foodstuffs.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDry; ISO 1183
Water Absorption 8.0 %Sim. to ISO 62
Moisture Absorption 2.00 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 80.0 MPaConditioned; ISO 2039-1
 140 MPaDry; ISO 2039-1
Tensile Strength, Yield 55.0 MPaConditioned; ISO 527-1/-2
 80.0 MPaDry; ISO 527-1/-2
Elongation at Break 5.0 %Nominal, Dry; ISO 527-1/-2
 >= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 4.0 %Dry; ISO 527-1/-2
 15 %Conditioned; ISO 527-1/-2
Tensile Modulus 1400 MPaConditioned; ISO 527-1/-2
 3300 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 80.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 80.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 3.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 5.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+12 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 25.0 kV/mmConditioned; IEC 60243-1
 27.0 kV/mmDry; IEC 60243-1
Comparative Tracking Index 600 VDry; IEC 60112
 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°CISO 11359-1/-2
Melting Point 260 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 70.0 - 100 °CLong Term; ISO 2578
 220 °CShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 200 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Compliance PropertiesOriginal ValueComments
FDA YesFood contact
 
Descriptive Properties
Food contactEU Requirements
FormGranules
Industry & Consumer goodsHousewares
 Sports & Leisure
PackagingMedical packaging
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® C31 01 PA6/66
EMS-Grivory Grilon® TSS PA666
BASF Ultramid® C33 01 PA66/6 (Conditioned)
Akro-Plastic Akromid® C3 1 (4546) PA66/6 Conditioned
BASF Ultramid® C3U PA66/6 (Conditioned)

PGRH301 / 157010

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.