Grade N01N-00 is a high stiffness, impact copolymer specially designed for freezer-to-microwave performance. This extrusion grade resin exhibits an excellent balance of impact and stiffness properties, and combines high heat resistance with good gloss and thermoformability. This grade meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Applications:- Food service trays, containers
- Rigid packaging
Benefits:- Very broad temperature performance range
- High stiffness
- Low temperature impact
- Thermoformability
|
Excellent balance of impact and stiffness properties |