MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Sclair® 99K Homopolymer HDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: 99K complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals' polyethylene resins are chemically and biologically inert.

Features: Excellent processability, Excellent Stretchability, High stiffness, Superior strength, Low gel

Additives: Process stabilizer, Process aid

Applications: Industrial woven bags, Tarpaulins

Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and a 35-mil die gap at a blowup ratio of 2.5:1, but are dependant on operating conditions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.962 g/ccASTM D 792
Thickness 38.0 microns
Melt Flow 0.72 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 69ASTM D 2240
Film Tensile Strength at Yield, MD 27.0 MPaASTM D 882
Film Tensile Strength at Yield, TD 22.0 MPaASTM D 882
Film Tensile Strength at Break, MD 39.0 MPaASTM D 882
Film Tensile Strength at Break, TD 22.0 MPaASTM D 882
1% Secant Modulus, MD 830 MPaASTM D 882
1% Secant Modulus, TD 1330 MPaASTM D 882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 128 °CASTM D 1525
 
Optical PropertiesOriginal ValueComments
Haze 78 %ASTM D 1003
Gloss 5.0 %at 45°; ASTM D 2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 230 °CRecommended
Blow-up Ratio (BUR) 2.5 - 4.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil HD 7957.04 High Density Polyethylene (HDPE), Film Grade
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film
LyondellBasell Alathon L4550 High Denisty Polyethylene
Lotte Chemical Titan TITANEX® HF0961 High density polyethylene Hexene-1 resin
ExxonMobil HD 7960.13 HMW Blown Film Resin

PNOV865 / 108472

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.