Chromium alloyed steel Typical applications for Ramax® HH are: holders and bolsters for plastic molds, plastic and rubber molds with low requirements on polishability, and dies for plastic extrusion. RAMAX® HH is characterized by: - Excellent machinability
- Good corrosion resistance
- Good hardenability
- Uniform hardness in all directions
- Good indentation resistance
|