MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Quaker Quintolubric® 822-450 Fire Resistant HFD-U Hydraulic Fluid
Categories: Fluid

Material Notes: Benefits:
  • Good fire-resistant properties
  • FM Approved as a less hazardous hydraulic fluid
  • Approved by MSHA Approval No. 30-20-3
  • Excellent lubrication properties
  • Excellent shear stability
  • Compatible with most standard seal materials
  • Low human and ecological toxicity
  • Cleanliness: max. NAS 1638 class 6 in bulk, max. NAS 1638 class 7 in containers/drums
  • Product is >90% biodegradable according to CEC L-33-T-82
  • Energy saving because of low density compared to other HFD type fluid
  • Excellent cost and quality balance for selected systems
Applications: QUINTOLUBRIC® 822-450 was designed to replace anti-wear, mineral oil-based hydraulic fluid used in fire hazardous and environmentally sensitive hydraulic applications without compromising overall hydraulic system operation. QUINTOLUBRIC® 822-450 is based on synthetic esters and contains an optimized additive package. It does not contain water, phosphate esters or chlorinated hydrocarbons.The product is widely used over many types of industries. Major applications include the Steel industry, Non-ferrous industry, Glass industry, Mobile equipment and Mining.

Information provided by Quaker

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/cc
@Temperature 50.0 °C
ASTM D1298
 0.922 g/cc
@Temperature 25.0 °C
ASTM D1298
Viscosity Measurement 145Index; ASTM D2270
Kinematic Viscosity 100 cStASTM D445
Viscosity Measure 1050 cSt
@Temperature 0.000 °C
Kinematic; ASTM D445
Kinematic Viscosity at 40°C (104°F) 30 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 14 cStASTM D445
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 2.0[mg KOH/g}; ASTM D974
 
Thermal PropertiesOriginal ValueComments
Pour Point <= -26.0 °CASTM D97
Flash Point >= 260 °CASTM D92
 
Descriptive Properties
AppearanceLight amber, clear fluid
Fire Point>340°CASTM D92
Pump Test<20 mg wearring plus vanes, ASTM D2282
Water Separability40-40-0 ml-ml-mloil-water-emulsion, 30 min, ASTM D1401

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WQUAK009 / 184995

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.