MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips Sumika Marlex® HGZ-180 Polypropylene Homopolymer, General Purpose Fiber Grade, Low Gas Fading  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: This material meets FDA regulation CFR 21 177.1520 and is suitable for food packaging applications.

Applications:
  • Bulked continuous filament
  • Craft yarn
  • Nonwoven fabrics

Information provided by Chevron Phillips.

Phillips Sumika Polypropylene Company has been shut down, as announced in 2011.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.909 g/ccInjection molded specimen; ASTM D1505
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 74Injection molded specimen; ASTM D785
Tensile Strength, Yield 34.0 MPa2 in/min, injection molded, type 1 specimen; ASTM D638
Flexural Modulus 1.861 GPaInjection molded specimen, 0.5 in/min, Tangent method; ASTM D790
Izod Impact, Notched 16.0 J/m
@Temperature 23.0 °C
injection molded specimen; ASTM D256
Izod Impact, Unnotched 16.0 ft-lb/in
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 104 °CInjection molded specimen; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °CInjection molded specimen; ASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
processFiber

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phillips Sumika Marlex® HGN-200 Polypropylene Homopolymer, Nucleated
Phillips Sumika Marlex® HGL-200 Polypropylene Homopolymer, Antistatic
Chevron Phillips Marlex® HNZ-020 Polypropylene Extrusion/Blow-Molding Resin

PCHEVD094 / 20673

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.