AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable to simple shapes and thermo-formable to complex three-dimensional curves, and is nonfriable. AIREX® R63 is a core material for dynamically loaded and shock absorbing sandwich structures.Characteristics- Good impact strength (non-brittle failure mode)
- Easy to thermoform (cold and hot)
- Dimensionally stable
- Excellent fatigue resistance
- Outstanding core-to-skin adhesion
- Non biodegradable
- Good sound and thermal insulation
Applications- Marine: Hull bottoms, hull sides
- Road and Rail: Front-ends, side skirts, crash belts
- Aircraft: Explosion proof cargo containers
- Recreation: Surf boards, canoes, kayaks
- Industrial: Containers, shelters, helmets
|