MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Sinkral® B 4 Venezia Extrusion Grade ABS Polymer
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: B 4 Venezia is an extrusion grade developed for glossy applications. Easily extrudable even in large sheets, it has high gloss and high modulus.

Applications: It's used in sectors that need high gloss and good process ability.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Water Absorption 0.30 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D 570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cminternal method
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110ISO 2039/2
Tensile Strength 50.0 MPa50 mm/min; ASTM D 638
Elongation at Break 45 %50 mm/min; ASTM D 638
Flexural Strength 68.0 MPa2 mm/min; ASTM D 790
Flexural Modulus 2150 MPa2 mm/min; ASTM D 790
Izod Impact, Notched (ISO) 15.0 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
DIN 53453
 NB
@Temperature -40.0 °C
DIN 53453
Charpy Impact, Notched 12.0 kJ/m²DIN 53453
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+15 ohmDry; IEC 60093
Dielectric Constant 3.1
@Frequency 1000 Hz
Dry; IEC 60250
Dielectric Strength 30.0 kV/mmDry; IEC 60243
Dissipation Factor 0.015
@Frequency 1000 Hz
Dry; IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°CASTM D 696
Thermal Conductivity 0.170 W/m-KASTM C 177
Deflection Temperature at 1.8 MPa (264 psi) 104 °C120°C/h. Annealed; ASTM D 648
Vicat Softening Point 104 °C
@Load 5.10 kg
50°C/h; ISO 306/B 120
 109 °C
@Load 1.02 kg
120°C/h; ISO 306/A 120
Flammability Test 1.0
@Thickness 1.50 mm
internal test
Glow Wire Test 650 °C
@Thickness 3.00 mm
IEC 60695-2-1
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 230 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENF9904 / 265701

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.