MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Dowlex™ 2045.11S PE
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description:
  • For high speed, thin film applications
  • Additional thermal stability
  • Complies with US FDA 21 CRF 177.1520©3.2a
  • Complies with Canadian HPFB No Objection (with Limitations)
  • Complies EU, No 10/2011
  • Consult the regulations for complete details

Availability: Asia Pacific; Latin America; North America

Additive: Antiblock: 3000 ppm; Processing Aid: No; Slip: 1200 ppm

Agency Ratings: EU, No 10/2011; FDA 21 CRF 177.1520©3.2a; Canadian HPFB No Objection

Form: Pellets

Processing Method: Blown Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 3000 ppm
Slip Level 1200 ppm
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 7.00 lb (f)
Film Tensile Strength at Yield, MD 1940 psiASTM D882
Film Tensile Strength at Yield, TD 2050 psiASTM D882
Film Elongation at Break, MD 540 %ASTM D882
Film Elongation at Break, TD 660 %ASTM D882
1% Secant Modulus 30600 psiMD; ASTM D882
 33900 psiTD; ASTM D882
2% Secant Modulus 24900 psiMD; ASTM D882
 27400 psiTD; ASTM D882
Puncture Energy 11.0 in-lb
Elmendorf Tear Strength MD 440 gASTM D1922
Elmendorf Tear Strength TD 630 gASTM D1922
Dart Drop Test 180 gASTM D1709A
Film Tensile Strength at Break, MD 6690 psiASTM D882
Film Tensile Strength at Break, TD 5120 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 252 °F
Vicat Softening Point 219 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 20 %ASTM D1003
Gloss 34 %45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 420 °FExtrusion
Blow-up Ratio (BUR) 2.5
 
Descriptive Properties
Film Puncture Resistance75 ft-lb/in3
Film Toughness1330 ft-lb/in3MD, ASTM D882
 1370 ft-lb/in3TD, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF412 / 311105

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.