MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DESMODUR® MDQ23165 + BAYTEC® D22-70MF + BAYTEC® XL B (Catalyst SD6-2) 55 D Polyurethane, MDI-Ester
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccBAYTEC® XL B
 1.17 g/ccDESMODUR® MDQ23165
 1.17 g/ccBAYTEC® D22-70MF
 1.26 g/cc
Viscosity 50 cPBAYTEC® XL B
 650 cPBAYTEC® D22-70MF
 1000 cPDESMODUR® MDQ23165
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55DIN 53505
 51
@Temperature 80.0 °C
DIN 53505
 63
@Temperature -5.00 °C
DIN 53505
Tensile Strength at Break 33.0 MPaDIN 53504
Tensile Stress at Strain 13.4 MPa
@Strain 10 %
DIN 53504
Elongation at Break 600 %DIN 53504
100% Modulus 0.0162 GPa
@Strain 100 %
DIN 53504
200% Modulus 0.0171 GPa
@Strain 200 %
DIN 53504
300% Modulus 0.0188 GPa
@Strain 300 %
DIN 53504
Resilience 38[%]; DIN 53512
Tear Strength 668 pliwith nick; ISO 34-1
 822 pliwithout nick; ISO 34-1
Abrasion 45[mm3]; ISO 4649
 
Processing PropertiesOriginal ValueComments
Processing Temperature 35.0 °CDESMODUR® MDQ23165
 35.0 °CBAYTEC® XL B
 70.0 °CBAYTEC® D22-70MF
Mold Temperature 80.0 °C
Pot Life 2.50 min
 
Descriptive Properties
AppearanceliquidDESMODUR® MDQ23165
 solidBAYTEC® D22-70MF
 solidBAYTEC® XL B
Content0.3SD6-2 % / total (by weight), (catalyst at the head)
 100Parts by weight of prepolymer
 15.9Parts by weight of BAYTEC® XL B
 16.2-16.6%NCO
 30Parts by weight of BAYTEC® D22-70MF

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0455 / 202238

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.