MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lotus Nano Paint NAP 101 Nano-paint
Categories: Fluid

Material Notes: Description: Traffic marking nano-paints improved with nano-particles to get better performance in traffics on the road. Better mechanical properties, excellent traffic performance and more durability on the road are the results of applying nanotechnology in traffic marking paints.

Applications: Urban and inter-city

Information provided by Lotus Nanopaint

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 - 1.60 g/ccASTM D1475
Solids Content 51 - 55 %by Volume
 73 - 77 %by Weight; ASTM D1644
 
Processing PropertiesOriginal ValueComments
Dry Time 0.330 hour
@Temperature 25.0 °C
ASTM D711
 
Descriptive Properties
ColorWhite, Yellow, Red and BlueASTM EN 1439
Coverage8.7 m2/LiterASTM D344
CuringSolvent Evaporation
Direction Reflectance (%)~55%Colored, ASTM E97
 86White, ASTM E97
GlossOpaque
ResinAcrylic
Skiing Resistance (SRT)PassesASTM EN 1436
ThinnerLotus 65 B
Water ResistancePassesASTM D870

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTATP07 / 135225

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.