MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Meforex® 134a Ozone-Friendly CFC Replacement
Categories: Fluid

Material Notes: Formula: CH2FCF3; Name: 1,1,1,2 Tetrafluoroethane. Replaces CFC 12, R 500. Domestic refrigeration, commercial and automotive air-conditioning, polystyrene and polyurethanes foams, and pharmaceutical aerosol propellant.

Information provided by Solvay Solexis, Inc.

Key Words: CH2FCF3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/cc
@Temperature 25.0 °C
Liquid
Molecular Weight 102 g/mol
Vapor Pressure 6.66 bar
@Temperature 25.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 40.67 bar
Critical Temperature 101.1 °C
Critical Density 0.510 g/cc
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 217 J/gat Boiling Point
Melting Point -101 °Cat 1.013 bar
Boiling Point -26.2 °Cat 1.013 bar
 
Descriptive Properties
Flammability Range (vol%)None
Ozone Depletion Potential0Based on CFC11 = 1.0
Toxicity Level1000 ppmAllowed limit in work places, values suggested by AIHA (American Industrial Hygiene Association).

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ammonia, NH3
Solvay Chemicals SOLKANE® 134a Refrigerant
Honeywell Genetron® 134a Refrigerant
Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core
Beijing Evergrow Resources CFC-DDX-1000S Carbon Fiber Cloth

WAUSI05 / 74564

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.