SABIC® PPcompound 9135A is an elastomer-modified mineral filled Polypropylene with excellent impact and stiffness ratio. Typical material application are light esthetical automotive interior parts. It has a very high scratch resistance, no stickiness and a high flow. The material has anti static performance to reduce dust attraction.
SABIC®PPcompound 9135A is a designated automotive grade.
IMDS ID: 153097567Information provided by SABIC |