Riteflex XFR 655 is a thermoplastic polyester elastomer featuring a halogen-free flame redardant system and is UL certified to be V-0 at 1.5 mm in all colors. It has shore D hardness of 55 and an excellent balance of mechanical properties, flame retardant efficiency and processability.Information provided by Celanese |