MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotchkote™ EA5WB WB Epoxy Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: 3M Scotchkote WB Epoxy Coating EA5WB is a member of the expanding range of 3M Scotchkote high performance coating. It has been specifically developed for original equipment manufacture, particularly within the water industry. Scotchkote WB epoxy coating EA5WB is water borne coating for pumps, valves, and fittings providing corrosion resistance for steel, stainless steel and aluminum substitutes.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/cc
Solids Content 45 %
Volatile Organic Compounds (VOC) Content 120 g/l
Thickness 3.20 - 6.00 milDry
 7.20 - 13.2 milWet
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hourTouch Dry
 24.0 hourHard Dry
 168 hourFull Cure
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM35339 / 170086

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.