MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay AG-RHO™ FKC 1500 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Ag-RHO FKC 1500 is a unique surfactant for pesticide formulations, more specifically, a biological activator for glyphosate formulations. AG-RHO FKC 1500 is compatible with high-electrolyte solutions and stable in various salts of glyphosate

Chemical Name: PROPRIETARY BLEND

Solubility: Readily soluble in water. Soluble in water miscible solvents

Stability: Stable in hypochlorite and hydrogen peroxide solutions. Stable in the presence of acid solutions and high concentrations of alkaline builders. Stable to hard water.

Compatibility: Compatible with all other types of surfactants.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: AG-RHO® FKC 1500 is a unique surfactant for pesticide formulations, more specifically, a biological activator for glyphosate formulations. AG-RHO® FKC 1500 is compatible with high-electrolyte solutions and stable in various salts of glyphosate. This high-performance proprietary blend is bio-degradable and patented.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 66 - 72 %Karl Fisher; RP-0327
pH 6.0 - 8.01% Solution; RP-0420
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 100 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceColorless to Amber LiquidRP-0064

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay AG-RHO™ FKC 1000 Surfactant
Solvay ALKAMULS® S 20 Surfactant
Solvay AG-RHO™ GPA Surfactant
Solvay AG-RHO™ FM 3896 Surfactant
Solvay AG-RHO™ EM 30 Surfactant

WRHOD011 / 137241

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.