MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC VALOX™ 310 PBT (Americas)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Unreinforced, general purpose. Typical viscosity 5000-7000.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
 1.31 g/ccASTM D792
Water Absorption 0.080 %24 hours; ASTM D570
Viscosity 600000 cPmelt; SABIC method
Linear Mold Shrinkage, Flow 0.0090 - 0.016 cm/cm
@Thickness 0.750 - 2.30 mm
SABIC method
 0.015 - 0.023 cm/cm
@Thickness 2.30 - 4.60 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.010 - 0.017 cm/cm
@Thickness 0.750 - 2.30 mm
SABIC method
 0.016 - 0.024 cm/cm
@Thickness 2.30 - 4.60 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 117ASTM D785
Tensile Strength at Break 51.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 51.0 MPa50 mm/min; ASTM D638
Elongation at Break 300 %50 mm/min; ASTM D638
Flexural Strength 82.0 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Yield Strength 82.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2340 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 53.0 J/mASTM D256
Izod Impact, Unnotched 1602 J/mASTM D4812
Gardner Impact 40.0 JASTM D3029
 40.0 JASTM D3029
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 4.00e+16 ohm-cmASTM D257
Dielectric Constant 3.1
@Frequency 1e+6 Hz
ASTM D150
 3.3
@Frequency 100 Hz
ASTM D150
Dielectric Strength 15.7 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
 15.7 kV/mm
@Thickness 3.20 mm
in air; ASTM D149
 23.2 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
 23.2 kV/mm
@Thickness 1.60 mm
in air; ASTM D149
Dissipation Factor 0.0020
@Frequency 100 Hz
ASTM D150
 0.020
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index >= 600 VUL 746A
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 81.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 139 µm/m-°C
@Temperature 60.0 - 138 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
UL RTI, Electrical 120 °CUL 746B
UL RTI, Mechanical with Impact 120 °CUL 746B
UL RTI, Mechanical without Impact 140 °CUL 746B
Flammability, UL94 HB
@Thickness 1.47 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 240 - 255 °CInjection Molding
Zone 1 230 - 250 °C
Zone 2 240 - 255 °C
Zone 3 245 - 260 °C
Melt Temperature 245 - 260 °C
Mold Temperature 50.0 - 75.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 12.0 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 80 %
Vent Depth 0.00130 - 0.00250 cm
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10213 / 243680

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.