General purpose, peroxide cured, Ethylene Propylene Terpolymer, 85-95 °IRHD. Terpolymer of ethylene, propylene and diene monomers. ASTM D2000/SAE J200 line call out M8CA910, A25, B35, C32, EA14, and F17. Applications: Excellent water and steam resistance with good compression set properties. Improved heat resistance compared to sulphur cured EPDM. Not oil resistant. |