MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Superior Flux Superior No. 43 Organic Acid Water-Soluble Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Formulated for tinning semi-conductor leads, component leads, diodes, wire, and piezo-electric parts.
  • Promotes outstanding solderability on Copper, Kovar, Alloy 42, Alloy 51, Electroless Nickel (EN), Beryllium Copper and other difficult to solder metals.
  • For use in automated and manual soldering processes.
  • Excellent flux for tin/lead and lead-free alloys.
  • Flux conforms to IPC-ANSI-J-STD-004, Type ORH1.
Description: Superior No. 43 is an organic acid (OA), water-soluble flux that contains an amino-acid/halide activator in combination with a fluoride that starts to clean metal surfaces at room temperature, reaching peak activity at 260°C/520°F. The flux wets very effectively and promotes outstanding solderability to a wide variety of difficult to- solder base metals, as well as badly oxidized metal surfaces. All post-solder residues are water-soluble.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.057 - 1.059 g/cc
pH 2.3 - 4.3
Surface Tension 35 dynes/cm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 95.0 - 315 °CSoldering Range
Shelf Life 2.00 Month
 
Descriptive Properties
Acid Equivalent1.0-1.6 gHydrogen/liter
Chloride Content17.5-25 gChlorine/liter
Fluorine Content23.2-33.2 gFluorine/liter
FormClear Colorless Liquid
ResiduesCompletely Water Soluble
Spread Factor>80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSFLUX018 / 185702

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.