MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zoltek™ PX35 UD500 Uni-Directional Carbon Fabric - Epoxy Composite
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Composite consists of 55 volume% fabric in an epoxy matrix. ZOLTEK PX35 Stitch-Bonded Uni-Directional Carbon Fabrics are produced from ZOLTEK PX35 50K Continuous Tow Carbon Fiber. Unique fiber spreading techniques are utilized to obtain a wide range of UD fabric weights for a varied set of composite part applications. Quick composite part build-up is cost effectively achieved with the diverse weight range of low-cost carbon fabric products.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1400 MPaDIN EN ISO 527
Tensile Modulus 119 GPaDIN EN ISO 527
Flexural Strength 187000 psiDIN EN ISO 14125
Flexural Modulus 112 GPaDIN EN ISO 14125
Compressive Strength 980 MPaDIN EN ISO 14126
Compressive Modulus 118 GPaDIN EN ISO 14126
 
Descriptive Properties
Fabric Component: 0° Carbon Zoltek PX35 50K (g/m2)500
Fabric Component: 90° Glass 34 dtex (g/m2)10
Fabric Component: Polyester Stitch 76 dtex (g/m2)6
Total Fabric Weight (g/m2)516

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zoltek™ PX35 UD900V Uni-Directional Carbon Fabric
Zoltek™ PX35 UD600 Uni-Directional Carbon Fabric - Epoxy Composite
Zoltek™ PX35 UD300 Uni-Directional Carbon Fabric - Epoxy Composite
Zoltek™ PX35 UD150 Uni-Directional Carbon Fabric - Epoxy Composite
Zoltek™ PX35 Multi-Directional Carbon Fiber Fabric

PZOL805 / 232272

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.