MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® 7105 Film Grade LLDPE Hexene Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: This LLDPE is tailored for blown film applications that require: Excellent toughness properties; Good drawdown; Good processing characteristics; Use alone or in co extrusions; blends with other polyolefins

Typical blown film applications include:; High strength industrial film; General purpose packaging.

information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D1505
Thickness 1.00 milAs Tested
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 0.000 ppm
Slip Level 0.000 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 450 %
@Thickness 0.0254 mm
ASTM D882
Film Elongation at Break, TD 750 %
@Thickness 0.0254 mm
ASTM D882
Coefficient of Friction >= 1.0ASTM D1894
Elmendorf Tear Strength MD 500 g
@Thickness 0.0254 mm
ASTM D1922
Elmendorf Tear Strength TD 850 g
@Thickness 0.0254 mm
ASTM D1922
Elmendorf Tear Strength, MD 500 g/mil
@Thickness 0.0254 mm
ASTM D1922
Elmendorf Tear Strength, TD 850 g/mil
@Thickness 0.0254 mm
ASTM D1922
Dart Drop 400 g/mil
@Thickness 0.0254 mm
ASTM D1709
Dart Drop Test 400 g
@Thickness 0.0254 mm
ASTM D1709
Film Tensile Strength at Break, MD 72.0 MPa
@Thickness 0.0254 mm
ASTM D882
Film Tensile Strength at Break, TD 52.0 MPa
@Thickness 0.0254 mm
ASTM D882
1% Secant Modulus, MD 221 MPa
@Thickness 0.0254 mm
ASTM D882
1% Secant Modulus, TD 262 MPa
@Thickness 0.0254 mm
ASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 12 %
@Thickness 0.0254 mm
ASTM D1003
Gloss 90 %
@Thickness 0.0254 mm
60°; ASTM D2457
 
Descriptive Properties
Process AidNone

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEVC8905 / 241988

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.