MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Alpha-2 Titanium Aluminide, Ti3Al
Categories: Metal; Intermetallic

Material Notes: Intermetallic aluminides have good mechanical properties and stability to be used in high temperature environments. A thin protective Al2O3 coating forms to provide oxidative stability. A range of stoichiometries is possible through elemental substitutions. Researchers are examining titanium aluminide applications in fields such as jet engine turbines because of their high temperature properties and low density.

May be cast. Difficult to process by ingot metallurgy, forging, or sheet rolling.

Key Words: Ti3Al
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 800 - 1140 MPa
Tensile Strength, Yield 700 - 990 MPa
Elongation at Break 0.00 - 10 %
Modulus of Elasticity 145 GPa
 
Thermal PropertiesOriginal ValueComments
Melting Point 1600 °C
Maximum Service Temperature, Air 650 °COxidation Limit
Maximum Service Temperature, Inert 760 °CCreep Limit
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 15.8 %by weight
Titanium, Ti 84.2 %by weight
 
Descriptive Properties
Critical Ordering Temperature1100°C
Crystal StructureD019Ordered HCP

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gamma Titanium Aluminide, TiAl
Titanium Aluminide, TiAl3
Ti-24Al-11Nb Titanium Aluminide
Titanium Ti-13V-11Cr-3Al; (Ti-13-11-3) Annealed 850°C (1560°F) + Aged 510°C 8 hr
Titanium, Ti

MIAL000 / 12198

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.