MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arkema Kynar Flex® Ultraflex B PVDF
Material Notes:

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 - 1.83 g/ccASTM D792
Density 1.77 g/ccISO 1183
Water Absorption 0.030 %Dry; Sim. to ISO 62
 <= 0.040 %ASTM D570
Viscosity 1.20e+6 - 2.00e+6 cP
@Shear Rate 100 1/s,
Temperature 230 °C
Melt; ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 35 - 43ASTM D2240
Tensile Strength at Break 8.96 - 20.7 MPaASTM D638
Tensile Strength, Yield 6.50 MPaDry; ISO 527-1/-2
 4.83 - 8.27 MPaASTM D638
Elongation at Break >= 50 %Dry; ISO 527-1/-2
 <= 500 %ASTM D638
Elongation at Yield 20 %Dry; ISO 527-1/-2
 25 - 35 %ASTM D638
Tensile Modulus 34.5 - 103 MPaASTM D638
 80.0 MPaDry; ISO 527-1/-2
Flexural Modulus 68.9 - 138 MPaASTM D790
Charpy Impact, Notched NB
@Temperature 23.0 °C
Dry; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 101 °C10°C/min; Dry; ISO 11357-1/-3
 92.0 - 112 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °CDry; ISO 75-1/-2
Glass Transition Temp, Tg -40.0 °CASTM D7028
Oxygen Index >= 40 %
 40 %Dry; ISO 4589-1/-2
 
Descriptive Properties
Form as DeliveredCrumb
Moisture SensitiveNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Kynar Flex® PPA 2200 PVDF
Arkema Kynar Flex® 3030-10 PVDF
Arkema KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Arkema Kynar Flex® PPA 5300 PVDF
Arkema KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding

PARKF724 / 193526

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.