MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Zotefoams ZOTEK® F OSU Semi-Rigid PVDF Foam
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: Zotek® F OSU is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.

This grade is ideal for soft trim in combination with leathers, textiles and decorative laminates, including low FST cores for composites and divider panels.

Information provided by Zotefoams

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0340 g/ccISO 845
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 0.417 MPaISO 1798
Elongation at Break 74 %
Compressive Yield Strength 0.0740 MPa
@Strain 25 %
ISO 7214
Tear Strength 0.823 kN/mISO 8067
Compression Set 50 %
@Time 79200 sec,
Strain 50 %
0.5 hr recovery; ISO 7214
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0321 W/m-Kmean temp of 0°C; ISO 8301
 0.0370 W/m-Kmean temp of 50°C; ISO 8301
 0.0407 W/m-Kmean temp of 83°C; ISO 8301
Maximum Service Temperature, Air 155 °C
 
Descriptive Properties
FlammabilityHeat Release: FAR/CS 25.853, 2 min total30.2 kWmin/m2
 Heat Release: FAR/CS 25.853, Peak35 kW/m2at 1 in
 Toxic Gas Emission: ABD0031Pass at 25 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Carbon Nanofoam
MarkeTech Silica Aerogel
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Overview of materials for Silicone Foam
Overview of materials for Expanded Polystyrene (EPS)

PZOTEF960 / 150716

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.