MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Rogers Corporation Bisco™ HT-800 Cellular Silicone Foam
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Foam

Material Notes: Medium grade silicon sponge. UL recognized for flame retardance and gasketing.

Applications: HID (High Intensity Discharge) lighting fixture gaskets, Battery cushion in hand-held electronic products, Seals in equipment access panels, Electrical and electronic enclosure gaskets, Solder gun insulation pads for work stations

Gasketing and sealing rating is JMLU-2 (Listed) per UL 157. No UV degradation per SAE J-1960. Ozone effect rating is 0 (no cracks) per ASTM D-1171. No staining per ASTM D-925(A). Passes AMS-3568 corrosion resistance. Passes SMP-800-C & BSS toxic gas emission rating. Passes hot flex at 230°C (446°F) per ASTM D-573.

General BISCO™ silicone information: BISCO™ Cellular Silicones are used as sealing cushioning, vibration isolation, insulation, and thermal management gaskets. Their resistance to environmental extremes, mechanical resilience, and safety features lead to their use in transportation equipment, communications and electrical enclosures, electronic products and components, industrial machinery, and appliances.

Data provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 g/ccASTM D3574
Water Absorption 1.4 %ASTM D471
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 0.310 MPaASTM D412
Elongation at Break 80 %ASTM D412
Compressive Yield Strength 0.0550 MPaat 25% deflection; ASTM D1056
Compression Set <= 1.0 %
@Temperature 70.0 °C
ASTM D1056
 <= 5.0 %
@Temperature 100 °C
ASTM D1056
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Constant 1.42
Dielectric Strength 3.60 kV/mmASTM D150
Arc Resistance 92 secDry; ASTM D495
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0900 W/m-KASTM C158
Maximum Service Temperature, Air 200 °CRecommended use; SAE J-2236
 250 °CIntermittent; Rogers internal test
Minimum Service Temperature, Air -55.0 °CRecommended use; SAE J-2236
Brittleness Temperature -55.0 °CLow temp embrittlement; ASTM D746(B)
Flammability, UL94 V-0Listed (may vary with thickness, color, density)
Flame Spread Index <= 25IS; ASTM E162
Smoke Density <= 20 minDX at 1.5 minutes; ASTM E662
 <= 50 minDX at 4 minutes; ASTM E662
Oxygen Index 40 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Nitride
Silicon Nitride, HIP-RBSN
Silicon Nitride, HIP-SN
Silicon Nitride, HPSN
Silicon Nitride, RBSN

PROGBI6 / 66287

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.