MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Plaskolite Optix® CP-927HF PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: Availability: Europe; North America

Features: Chemical Resistant; Electrically Insulating; Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Weather Resistance; High Clarity; High Flow; Low Odor; Low to No Taste; Machinable

Appearance: Colors Available

Form: Pellets

Processing Method: Injection Molding

Information provided by Plaskolite, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccASTM D792
Water Absorption 0.30 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cmASTM D955
Melt Flow 11 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 53ASTM D785
Tensile Strength at Break 7300 psiASTM D638
Elongation at Break 18 %ASTM D638
Tensile Modulus 290000 psiASTM D638
Flexural Strength 11000 psiASTM D790
Flexural Modulus 310000 psiASTM D790
Izod Impact, Notched 1.00 ft-lb/inASTM D256
Izod Impact, Unnotched 13.0 ft-lb/inASTM D4812
Gardner Impact 25.0 in-lbASTM D3029
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 42.0 µin/in-°F
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 172 °FUnannealed; ASTM D648
Vicat Softening Point 200 °FASTM D1525
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ASTM D542
Haze 2.0 %ASTM D1003
Transmission, Visible 91 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 400 - 480 °F
Middle Barrel Temperature 410 - 490 °F
Front Barrel Temperature 420 - 500 °F
Nozzle Temperature 410 - 500 °F
Melt Temperature 410 - 480 °F
Mold Temperature 120 - 175 °F
Drying Temperature 150 - 165 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPLASKO837 / 311530

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.