Description: Unreinforced and modified copolyamide 66/6, heat stabilized, with improved impact resistance, for injection molding. Available in: Europe Product Applications: TECHNYL B 238 is particularly recommended for applications where high thermal stress rates and good impact resistance are required, also for parts which could break during assembly or parts used at low humidity level. This grade is commonly used in: automotive industry for under bonnet fasteners. This product is available in black. DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe. |