MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Irathane Futura® IRABOND UU52 Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: A two component spray applied intercoat adhesive used in conjunction with Irabond 9924 when bonding hot processed polyurethane, eg 2855, to metal.

RECOMMENDED APPLICATIONS: Can also be used in conjunction with some Futura hot spray applied coatings to give improved adhesion in place of Irabond UU55. Can also be suitable when bonding to a cured rubber substrate, with Irabond RU80, as required.

FEATURES: • 2K system ensures full cure even when applied in a moisture free environment.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 17 %± 5%. By volume, component B
 
Thermal PropertiesOriginal ValueComments
Flash Point 87.8 °FComponent A
 87.8 °FMixed
 111 °FComponent B
 
Processing PropertiesOriginal ValueComments
Pot Life <= 480 min
@Temperature 30.0 °C
 <= 720 min
@Temperature 10.0 °C
Shelf Life 12.0 Month
@Temperature 22.0 °C
In original unopened container in dry environment.
 
Descriptive Properties
ColorColorlessComponent A
 ColorlessComponent B
 ColorlessMixed
Coverage5-7m²/L
Mix Ratio by volume1:1Component A: Component B
Mix Ratio by weight1:1Component A: Component B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWI9239 / 239748

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.