MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sterigenics Raprex® R-200 Branched High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Applications: Injection Molding and Extrusion

RAPREX® R-200 is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique branched structure. This structure is achieved through irradiation of the polymer. It is a thermoplastic and is fully recyclable. Due to its high molecular weight and shear sensitivity, RAPREX® R-200 is used for injection molding. Because of its high melt strength, it is also used for films, extrusion coating and foam applications. Raprex® R-200 contains a robust stabilization package providing excellent melt stability as well as long-term heat aging.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D792
High Load Melt Index 9.1 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
Melt Index of Compound 1.1 g/10 min
@Load 10.0 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 21.0 MPaASTM D638
Tensile Strength, Yield 40.0 MPaASTM D638
Elongation at Break 21 %ASTM D638
Elongation at Yield 9.0 %ASTM D638
Flexural Modulus 1.24 GPaASTM D790
Izod Impact, Notched NBASTM D256
 2.60 J/cm
@Temperature -40.0 °C
Partial Break; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -75.0 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 2652 Polycarbonate
Borealis FL5580 High Density Polyethylene
Asahi Kasei Leona® 1402F Nylon 66
Techmer ES Luriblend® PE 5903
Sterigenics Raprex® R200D Branched High Density Polyethylene

PRAPREX7 / 65283

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.