MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Phillips 66 Syncon® 68 Synthetic AW Hydraulic Fluid 68
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Description: Conoco Syncon Synthetic AW Hydraulic Fluid is a synthetic polyalphaolefin (PAO) antiwear fluid for hydraulic systems that operate at extreme temperatures. It is available in four ISO viscosity grades: 22, 32, 46 and 68.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.08 lb/gal
Viscosity Measurement 145Viscosity Index
Saybolt Viscosity at 100°F 315 SUS
Saybolt Viscosity at 210°F 60 SUS
Kinematic Viscosity at 40°C (104°F) 68 cSt
Kinematic Viscosity at 100°C (212°F) 10.3 cSt
ASTM Color 1.5
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.70
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 40.0 kV/mmNo thickness given
 
Thermal PropertiesOriginal ValueComments
Pour Point -65.0 °F
Flash Point 510 °F
 
Descriptive Properties
ASTM Rust A&BPass
Copper Corrosion1A
Emulsion Characteristics (40-37-3)Max 10 minutes
Vickers 35VQ-25 Pump TestPass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON167 / 75204

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.