MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DIAB ProBalsa® PB Standard Balsa Wood
Categories: Other Engineering Material; Composite Core Material; Wood and Natural Products; Wood

Material Notes: ProBalsa is a high quality composite core material made from end-grain balsa wood. The end grain, micro-honeycomb structure offers exceptional shear and compressive strength. In addition ProBalsa offers good fatigue properties, high thermal and sound insulation and low FST properties.

ProBalsa is best suited for dynamic structures where performance and efficiency are paramount. All ProBalsa core materials are particularly easy to work using conventional woodworking tools. They can be drilled, milled, turned and sawn to close tolerances. ProBalsa can be used in hand lay-up, vacuum bag and infusion applications. It is also suitable for elevated temperature cure prepreg systems. ProBalsa Plus is a premium version of ProBalsa where the surface is micro sanded and treated with a special surface primer to reduce resin absorption during lamination.

Information Provided by DIAB

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.155 g/ccASTM C271
Moisture Absorption at Equilibrium 12 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 13.5 MPaASTM C297
Compressive Strength 12.7 MPaASTM C365
Compressive Modulus 4100 MPaASTM C365
Shear Modulus 0.166 GPaASTM C273
Shear Strength 3.00 MPaASTM C273
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.10 µm/m-°CLongitudinal (Moisture changes are more impactful than CTE); ASTM D696
 4.60 µm/m-°CRadial (Moisture changes are more impactful than CTE); ASTM D696
 6.80 µm/m-°CTangential (Moisture changes are more impactful than CTE); ASTM D696
Thermal Conductivity 0.0640 W/m-K
@Temperature 10.0 °C
ASTM C377
Insulation R Value 1.1
@Thickness 12.0 mm
Based on +10°K factor
 2.3
@Thickness 25.0 mm
Based on +10°K factor
 4.5
@Thickness 51.0 mm
Based on +10°K factor

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DIAB ProBalsa® LD7 Light Weight Balsa Wood
American Balsa Wood
Tropical Balsa Wood
Carbon-Core Carbon Balsa Wood
DIAB ProBalsa® HW Heavy Weight Balsa Wood

PDIAA937 / 99175

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.