STYRON® 615 APR is a general purpose easy flow resin typically used for medical, pharmaceutical and thin-walled parts. It is an excellent resin for blending with K-Resin (K-Resin is a trademark of Phillips 66 Company). When used unmodified for the manufacture of food contact articles STYRON 615 APR complies with the US Food, Drug and Cosmetic Act and Food Additive Regulations 21 CFR 177.1640. The regulations should be consulted for complete details. Data provided by Dow Chemical. Americas Styrenics was formed in 2008 as a joint venture between Dow Chemical and Chevron Phillips Chemical Company. Styron was a Dow trade name before the JV formation. |