MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Kohesi Bond KB 1372 SC Two component, thermally conductive and chemically resistant epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Product Highlights:
  • Exceptionally high Tg
  • Very good flow properties
  • Superior chemical resistance
  • Long working life at room temperature
  • Exceptional electrical insulation properties
  • Phenomenal abrasion resistance
Kohesi Bond KB 1372 SC is a two component, heat curing epoxy system suitable for bonding, sealing, coating, potting and encapsulation. It has a convenient 10:1 (Part A: Part B) mix ratio by weight. This epoxy system offers a high glass transition temperature (Tg) of > 172°C. It rapidly cures at moderately elevated temperatures and can achieve even faster cures at higher temperatures. It takes 4 - 6 hours to cure at 70°C, 20 - 40 minutes at 100°C and 10 minutes at 125°C. Kb 1372 SC is an silicon carbide filled system, offering first-rate abrasion resistance. It offers very long working life at room temperature, allowing to bond and pot large parts. It has an extensive service temperature range of -50°C to +230°C. This adhesive fosters outstanding mechanical strength properties, along with dimensional stability. KB 1372 SC adheres well to a wide variety of substrates including metals, ceramics, most plastics and glass. In addition to superior electrical insulation, it also offers excellent chemical resistance to a variety of acids, bases, solvents and other chemicals. Part A and Part B are dark gray in color. KB 1372 SC is widely used in applications requiring excellent chemical resistance at elevated temperatures, long open time and very high abrasion resistance.

Typical Applications:

  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors: Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 2000 - 5000 cPMixed
 6000 - 10000 cPPart B
 45000 - 65000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 80
Tensile Strength 8600 psi
Tensile Modulus 510000 - 550000 psi
Adhesive Bond Strength >= 2500 psiTensile Lap Shear, Al/Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 3.26
@Frequency 60 Hz
Dielectric Strength 450 V/mil
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 230 °C
Minimum Service Temperature, Air -50.0 °C
Glass Transition Temp, Tg >= 172 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 - 6.00 hour
@Temperature 60.0 - 70.0 °C
Option 3
 10.0 min
@Temperature 125 °C
Option 2
 20.0 - 40.0 min
@Temperature 80.0 - 100 °C
Option 1
Working Life >= 720 min100 g of mixed epoxy
Shelf Life 12.0 Monthin original unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKOHESI935 / 249114

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.