MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® LF-1930 HS BK545-9 Polyphthalamide (PPA), 30% Long Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: Amodel® LF-1930 HS BK545-9 is 30% long glass fiber reinforced, easy-flowing PPA which can be processed on most injection molding machines.

This material achieves extremely high mechanical and thermal properties, in combination with ease of processing and fast cycle times. It exhibits high strength, stiffness and impact strength at high temperatures; excellent creep and fatigue resistance; isotropic mechanical properties and reduced anisotropic shrinkage; high shear strength and high burst pressure; and an excellent surface finish.

Creep Resistant; Electrically Insulating; Fatigue Resistant; High Impact Resistance; High Rigidity; High Stiffness; High Tensile Strength; Low CLTE; Low Warpage

Uses: Aircraft Applications; Automotive Applications; Automotive Instrument Panel; Gears

Availability: Europe

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.44 g/ccISO 1183
 1.44 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 200 MPaISO 527-2
Elongation at Break 2.0 %ISO 527-2
Tensile Modulus 11000 MPaISO 527-2
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature 23.0 °C
ISO 179
Charpy Impact, Notched 20.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 300 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 285 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 320 - 340 °C
Middle Barrel Temperature 325 - 340 °C
Front Barrel Temperature 325 - 340 °C
Nozzle Temperature 325 - 345 °C
Melt Temperature <= 345 °C
Mold Temperature 130 - 160 °C
Drying Temperature 120 °C
@Time 14400 sec
Moisture Content 0.060 %
 
Descriptive Properties
ColorBlack
FormsPellets
Suggested Max Regrind (%)20

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Amodel® FC-1150 Polyphthalamide (PPA), 50% Glass Fiber
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS)
DuPont Mobility and Materials Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA)
Clariant Renol PPSSP0001 Polyphenylene Sulfide, Glass Fiber and Bead Filled
Clariant Renol PPA1100G50 Polyphthalamide, 50% Glass Fiber

PSOL8Y6089 / 193010

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.