MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials BETAFORCE™ 2817 V1 Polyurethane Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: 2-component polyurethane adhesive with short working time at room temperature, suitable for structural bonding.

Information provided by DuPont Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 - 1.19 g/cc
 1.41 - 1.45 g/cc
Viscosity Measurement 22 - 37
@Thickness 2.00 mm
g/min Extrusion Viscosity; Component A; 4bar
 20 - 40
@Thickness 2.00 mm
g/min Extrusion Viscosity; Component B; 4bar
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 23.0 MPaISO 527-1/-2
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °CTemperature stability
Minimum Service Temperature, Air -40.0 °CTemperature stability
 
Processing PropertiesOriginal ValueComments
Processing Temperature 18.0 - 28.0 °C
Tack-Free Time 8.00 - 10.0 min30 - 50 cm length adhesive beads
Shelf Life 6.00 Month
@Temperature 5.00 - 25.0 °C
 
Descriptive Properties
BasisPolyol and isocyanate
ColorBlack
 BlackComponent A
PolymerAdhesive
Regional AvailabilityAsia Pacific
 Europe
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDTF9016y / 295946

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.