MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Regal® Marine 77
Categories: Fluid; Lubricant

Material Notes: Texaco Regal Marine 77 delivers value through:
  • Long lubricant life because of selected base stocks and additives
  • Extreme pressure characteristics provide high film strength to protect gears and bearings engaged in severe, heavy-duty service.
  • MIL-L-17331H(SH) qualified - Meets stringent military specifications
  • High viscosity index - Minimal viscosity change in broad operating temperature range enhances lubricant film strength.

Texaco Regal Marine 77 was developed primarily as a circulating system oil for marine gear turbine sets.

Texaco Regal Marine 77 provides mild extreme pressure protection as well as resistance to rust, oxidation, corrosion, and foaming.

Texaco Regal Marine 77 has outstanding thermal and oxidation stability, which allows it to withstand the high temperatures, found in turbine bearing and gear lubrication.

The foam inhibition prevents the buildup of foam in the sump tank with possible vent pipe overflow.

Its excellent stability, high viscosity index, and rust and corrosion inhibition assures high film strength lubrication for gears and bearings, as well as rust and corrosion protection. Together, these qualities mean both long lubricant and equipment life.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 221506; MSDS Number: 8696

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 31.9 °
Viscosity Measurement 99Viscosity Index
Saybolt Viscosity at 100°F 415 SUS
Saybolt Viscosity at 210°F 59.1 SUS
Kinematic Viscosity at 40°C (104°F) 79.8 cSt
Kinematic Viscosity at 100°C (212°F) 9.7 cSt
Ash <= 0.0010 %Sulfated Ash
ASTM Color 0.50ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Acid Value 0.16mg KOH/g; ASTM D974
 
Thermal PropertiesOriginal ValueComments
Pour Point -12.0 °C
Flash Point 246 °C
 
Descriptive Properties
Conradson Carbon Residue, mass%0.1
Corrosion, Copper Strip13 h at 100°C
Rust PreventionPass48 h, Oil water washed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WTEXA159 / 77038

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.