MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 1001 FR A Polybutylene Terephthalate (PBT), Glass Fiber - Flame Retardant - UL94 V-0
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: RTP 1001 - 1005 FRA are a series of glass fiber reinforced, flame retardant PBT compounds. All are UL94 V-0 certified down to the 1/32" (0.8mm) thickness. These materials exhibit easy flow, excellent physical properties and good processing characteristics.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D 792
Filler Content 10 %Primary Additive
Water Absorption 0.070 %24 hrs @ 23°C; ASTM D 570
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D 785
Tensile Strength at Break 13500 psiASTM D 638
Elongation at Break 4.0 - 5.0 %ASTM D 638
Tensile Modulus 700 ksiASTM D 638
Flexural Strength 21000 psiASTM D 790
Flexural Modulus 600 ksiASTM D 790
Izod Impact, Notched 0.600 ft-lb/in
@Thickness 3.17 mm
D 256
Izod Impact, Unnotched 6.00 ft-lb/in
@Thickness 3.17 mm
ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D 257
Dielectric Constant 3.3
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 485 V/milShort Term; in oil; ASTM D 149
Dissipation Factor 0.020
@Frequency 1e+6 Hz
Dry; ASTM D 150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 380 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 340 °FASTM D 648
Flammability, UL94 V-0
@Thickness 0.7937 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 460 - 520 °F
Mold Temperature 175 - 225 °F
Drying Temperature 250 °F
Dry Time 4 hour
Moisture Content 0.030 %
Dew Point -20.0 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Novaduran® 5830GN6-40 Polybutylene Terephthalate
Mitsubishi Novaduran® 5010GNI-15AM Polybutylene Terephthalate
Mitsubishi Iupilon® MB 8700 PC/ABS
LG Chemical Lupox® GP-2301F General Purpose PBT, 30% Glass Fiber Reinforced, Flame Retardant
LATI Latamid 66 H2 G/25-V0CT4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant

PQZWA1943 / 90962

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.