BMC GP 400/20 is a bulk molding compound based on an unsaturated polyester resin, reinforced with glass fibers. This BMC has been developed for general purpose. Good mechanical properties and good flow are combined into the BMC GP 400/20. BMC GP 400/20 is formulated according to RoHS, REAC regulation (SVHC) and WEEE European legislation.Information provided by Polynt Composites. |