MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218G2 V50 Black 34N PA 66 50% Glass Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Description: TECHNYL® A 218G2 V50 Black 34N is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. The product is available in black color.

Key Properties: Excellent glycol resistance; Mechanical performance; Heat stabilized

Benefits: Technyl® A218G2 V50 Black 34N has been specially designed to improve its resistance to automotive cooling liquids, increasing lifetime of parts in permanent contact with such a liquid. Due to high content of glass fibers it offers also an excellent combination between thermal and mechanical properties

Applications: Technyl® A 218G2 V50 Black 34N is used in the automotive industry, for engine parts linked to cooling and heating systems that required a high level of mechanical resistance.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccISO 1183/A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 240 MPaISO 527 Type 1A
Elongation at Break 2.7 %ISO 527 Type 1A
Tensile Modulus 16200 MPaISO 527 Type 1A
Flexural Modulus 13500 MPaISO 178
Charpy Impact Unnotched 95.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75/Af
Flammability, UL94 HB
@Thickness 0.800 mm
ISO 1210
 HB
@Thickness 1.60 mm
ISO 1210
 HB
@Thickness 3.20 mm
ISO 1210
Glow Wire Test 650 °C
@Thickness 0.800 mm
Flammability Index; ISO 60695-2-12
 650 °C
@Thickness 1.60 mm
Flammability Index; ISO 60695-2-12
 650 °C
@Thickness 3.20 mm
Flammability Index; ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 280 °CCompression zone
 280 - 290 °CMixing zone
Feed Temperature 260 - 270 °C
Mold Temperature 60.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218G2 V50 Black 34N PA 66 50% Glass Reinforced, Conditioned
Domo TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY

PSOLVAY838 / 218566

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.