System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Denka GS-10 ABS Polymer
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Molded
Material Notes:
Semi-chemical resistance Grade. Used in a wide range of applications, including toys, home articles, home electric appliances, OA equipment, exterior and interior automotive parts, etc.
Information provided by Denka Company Limited.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.04
g/cc
ASTM D-792
1.05
g/cc
ISO 1183
Linear Mold Shrinkage
0.0040
-
0.0060
cm/cm
@Thickness 2.00 mm
DENKA Method
Melt Flow
22
g/10 min
@Load 9.99 kg,
Temperature 220 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
109
ISO 2039-2
116
ASTM D-785
Tensile Strength at Break
35.0
MPa
50 mm/min; ISO 527-1,-2
45.0
MPa
5 mm/min; ASTM D-638
Tensile Strength, Yield
47.0
MPa
50 mm/min; ISO 527-1,-2
Tensile Modulus
2450
MPa
1 mm/min; ISO 527-1, -2
Flexural Strength
72.0
MPa
15 mm/min; ASTM D-790
74.0
MPa
2 mm/min; ISO 178
Flexural Modulus
2300
MPa
2 mm/min; ISO 178
2400
MPa
15 mm/min; ASTM D-790
Izod Impact, Notched
226
J/m
ASTM D-256
Charpy Impact, Notched
21.0
kJ/m²
ISO 179
Electrical Properties
Original Value
Comments
Surface Resistance
>=
1.00e+16
ohm
50% RH; JIS K 6911
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
79.0
°C
Flatwise; ISO 75-1, -2
89.0
°C
Edgewise; ASTM D-648
Vicat Softening Point
100
°C
@Load 5.10 kg
ASTM D-1525
101
°C
@Load 5.10 kg
ISO 306
Flammability, UL94
HB
Processing Properties
Original Value
Comments
Processing Temperature
180
-
200
°C
Cylinder 1
190
-
220
°C
Cylinder 2
200
-
240
°C
Cylinder 3
Nozzle Temperature
200
-
235
°C
Mold Temperature
40.0
-
60.0
°C
Drying Temperature
80.0
-
85.0
°C
@Time 7200 - 10800 sec
Back Pressure
71.1
-
142
psi
Screw Speed
80
-
120
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PDENJ814 / 250158
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.