MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Inov Chem Donpanel 422 HCFC-141b Base blend polyols for PUR
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: DonPanel 422/ PUR blend polyols is a compound which consists of polyether polyols, surfactants, catalysts, HCFC-141B and flame retardant in a special ratio. The foam has good thermal insulation property, light in weight, high compression strength and flame retardant and other advantages. It is widely used to produce continuous sandwich panels, corrugated panels etc, which applies to make cold stores, cabinets, portable shelters and so on.

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 - 1.16 g/cc
Density 0.0280 - 0.0350 g/ccFree density, Manual Mix
 0.0330 - 0.0350 g/ccFree density, High temperature machine
 >= 0.0400 g/ccMold density; ASTM D 1622-08
Viscosity 300 - 400 cPDynamic
Storage Temperature 10.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 0.140 MPaGB/T 8813
Adhesive Bond Strength >= 0.120 MPaGB/T 16777
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.0220 W/m-K
@Temperature 15.0 °C
GB 3399
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 25.0 °CMaterial Temperature, Manual mix
 20.0 - 25.0 °CMaterial Temperature, High temperature machine
Mold Temperature 35.0 - 45.0 °CManual mixing
 35.0 - 45.0 °CHigh temperature machine
Gel Time 0.400 - 0.670 minHigh temperature machine
 0.500 - 1.00 minManual mixing
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceLight yellow transparent viscous liquid
Closed-cell rate=90%GB 10799
Cream time6-10 secHigh temperature machine
 8-16 secManual mixing
Dimensional stability=1.0%24h, -20?; GB/T8811
 =1.5%24h, 100?; GB/T8811
FlammabilityB2GB/T 8624
Hydroxyl value300-340 mgKOH/g
Recommended Ratio100:120-130DonPanel 422 blend polyols: Isocyanate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM019 / 312548

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.