MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Wall Colmonoy COLMONOY® 80 PTA Nickel-Base Hard Surfacing Composite Powder
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Tungsten Alloy

Material Notes: Colmonoy 80 PTA is a unique composite material containing a high volume percent of extremely abrasion resistant tungsten carbide particles (3500 DPH) in a soft (HRC 30) impact resistant nickel-base matrix alloy. The hard tungsten carbide particles provide abrasion resistance whereas the soft nickel matrix provides excellent ductility and impact resistance. The nickel alloy matrix and the tungsten carbide particles are uniquely matched so that a high volume percent of carbide grains are uniformly distributed throughout the matrix alloy.

Applications: Colmonoy 80PTA is specifically designed for PTA overlays that require a combination of high impact resistance and abrasion resistance. Typical applications include mining and drilling equipment, impact hammers, earthmoving and aggregate processing equipment and die plates. The nickel-base matrix alloy is specifically chosen to be soft (HRC30) and ductile to resist cracking under impact conditions. A high volume of carbide particles uniformly distributed in the matrix provides excellent abrasion resistance. Colmonoy 80PTA is not recommended for applications where the abrasive particles are extremely fine (less than 5 microns) or in a slurry form.

Information provided by Wall Colmonoy Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.80 g/ccapparent
 12.8 g/cctheoretical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 40single pass
 48double pass
 
Thermal PropertiesOriginal ValueComments
Melting Point 1820 - 2240 °F
Solidus 1820 °F
Liquidus 2240 °F
 
Component Elements PropertiesOriginal ValueComments
Boron, B 0.40 %
Carbon, C 3.8 %
Chromium, Cr 2.3 %
Iron, Fe 0.60 %
Nickel, Ni 35.3 %As Balance
Silicon, Si 1.6 %
Tungsten, W 56 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wall Colmonoy COLMONOY® 705 Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide
Wall Colmonoy COLMONOY® 4 Hard-Surfacing Alloy With Chromium Boride
Wall Colmonoy COLMONOY® 72 Nickel-Based Alloy With Chromium Carbide
Wall Colmonoy COLMONOY® 88 Hard-Surfacing Alloy
Wall Colmonoy COLMONOY® 635 Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide

NWALL18 / 19785

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.