MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling GLASTHERM HT250 Insulation Sheet
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: Glastherm Grade HT250 is a high compressive strength, heat-resistant composite material. It is ideal for insulation between the fold and the press or within the mold itself. Grade HT250 is asbestos-free and rugged to withstand rough handling during installation. Grade HT250 is employed to save energy during pressing and is mainly used in hydraulic, wood and tire presses.

Information provided by Glastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.00 g/ccASTM D-792
Water Absorption 0.15 %% by wt.; ASTM D-570
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 43500 psiASTM D-790
Compressive Strength 65200 psi
@Temperature 180 °C
ASTM D-695
 87000 psi
@Temperature 20.0 °C
ASTM D-695
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 12.0 kV/mmPerpendicular S/T in Air; ASTM D-149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.0 µm/m-°C
@Temperature 20.0 °C
Across Surface; ASTM D-696
 116 µm/m-°C
@Temperature 20.0 °C
Across Thickness; ASTM D-696
Thermal Conductivity 0.230 W/m-KASTM C-177
Maximum Service Temperature, Air 482 °F
 752 °F
 
Descriptive Properties
Standard ColorLight Green
Thickness Tolerance in± 0.00395-10mm
 ± 0.00611-20mm
Thickness Tolerance, %121-50mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gray Cast Iron, ASTM A 48 Class 40
Geon® Performance Solutions G26 Vinyl Compound - Flexible (FPVC)
Overview of materials for Gray Cast Iron
Röchling Glastic Grade HT250 Composite Material
Assab Steels 709M Machinery Steel

PGLASW8 / 41942

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.