Identification: SODIUM ALKYL DIPHENYL OXIDE SULFONATE CAS: 28519-02-0 Polarity: Strongly Anionic Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODACAL DBS is producer ABS type resins and various latex. It is used as Polymerization surfactant. In Oilfield it’s strongly anionic temperature is a stable foam booster. Information provided by Rhodia, Rhodia has been acquired by Solvay. |