MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Pearlthane® ECO 12T95 Thermoplastic Polyurethane
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type : Pearlthane® ECO 12T95 is a high performance bio-based thermoplastic polyurethane. With ca. 32% bio-based content.

Main Application : Injection Moulding

Special Features : Excellent mechanical properties and abrasion resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccISO 2781
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ISO 868
Tensile Strength 5220 psiISO 527-2/5A/500
Elongation at Break 415 %ISO 527-2/5A/500
50% Modulus 0.0100 GPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 0.0120 GPa
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 0.0280 GPa
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 811 pliISO 34-1B
Abrasion 28mm3 Loss; ISO 4649-A
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 107 °CISO 306
 
Processing PropertiesOriginal ValueComments
Feed Temperature 40.0 °C
Nozzle Temperature 215 - 225 °C
Zone 1 200 - 210 °C
Zone 2 205 - 215 °C
Zone 3 210 - 220 °C
Zone 4 210 - 220 °C
Dry Time 3.00 hour
@Temperature 100 °C
 
Descriptive Properties
Biobased Content (%)32
Compression Zone Temperature401°F
Metering Zone Temperature410°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Procom® D 1195 Polypropylene
Akro-Plastic Akromid® B3 GF 50 9 RM-M natural (3698) PA 6 Conditioned, 50% Glass Filled
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer

PMEQU970 / 109207

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.