Hostacom TRC 160N is a 15% talc filled PP copolymer, with excellent flowability, excellent impact/stiffness balance, good scratch resistance and outstanding surface appearance. This grade is delivered in customer customized colors, The product is available in different color matched, pellet form. This grade is delivered in C12616 color version. Applications: Interior TrimsInformation provided by LyondellBasell. |