MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daelim H&L Plavis-MS DF MoS2 Filled Aromatic Polyimide Bearing
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: Direct Formed. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.

General Plavis information for all grades:

PLAVIS polyimide has nitrogen bonded to 3 carbons is the critical part of the chain and imparts the plastic with remarkable features and benefits. PLAVIS is available as raw material or as molded parts, plates, and rods. PLAVIS isostatic molded rods have uniform properties in all directions.

Properties:

  • One of the highest temperature plastics in the world with a continuous operating temperature of 300°C. Well suited for cryogenic conditions
  • Retains high tensile strength and modulus even at high temperatures. Will not crack or creep under load.
  • Lowest out-gassing of any plastic at 300°C. Will not contaminate vacuum chamber process or products.
  • Grades are available for use at 1 million psi-fpm PV limit with lubrication, 300,000 psi-fpm PV limit without lubrication. Stable friction level.
  • Filled grades resistivity is tailorable.
  • Machines like brass-tiny and intricate features can be produced without cracking. Can be lapped to mirror finish.
Applications:
  • Flat Panel Display/Solar Cells:: Drying oven (HP/CP, Baking, IR) Glass support pins, Glass holders, Rollers; Cleaning EUV roller, Bearing; PVD/CVD Insulation parts Insert, Clamp, Bush, Caps, Susceptor pin, Ball bearing etc.; Etcher Screw, bolts. and Others Probe unit, station parts
  • Semiconductor: Wafer Processing Wafer clamp rings, Insulators, Screw & Fasteners, Vacuum pads, Alignment pins; Wafer handling, guides, and carriers, Vacuum pick up strips; IC handling & testing Die pick up collects, Test socket insulator
  • General Industry: Hot runner system Seal caps, Insulators; Plasma cutting torches parts Swirl rings, Insulator, Caps.; Heat resistance materials Bottle grippers, Conveyor tips; Scientific consumable parts GC/Mass ferrules, HPLC valve rotors; Textile Machines Valve seat, Bearing, Shedder Bushing
  • Automotive / Transportation:Transmissions Thrust Washers, Seal Rings, Valve Seats, Transmission Valve Balls, Check Valves; Electrical Motors Bushings, Washers, Thrust Plugs; Brakes Wear Pads, Valve Seats and Balls in ABS Systems; Fuel Systems Bushings, Seal Rings, Band Springs, Valve Seats; Turbo Chargers Ball Bearing Retainers, Wastegate Bushings; Vacuum Pump Vanes, Engine Belt Tensioners, Rubbing Blocks, Door Hinge Bushings, Gear Stick Rollers, Ignition Distributors, Constant Friction Pads for Split-Flywheels
  • Aerospace/Aircraft: Compressor Variable Vane Bushings and Washers, Aircraft Fan Thrust Reverser, Fan Blade Wear Strips, Locking Insert Nut, Fuel Line Spacer, Reciprocating Shaft Seal for Jet Engine Afterbunner Actuating System

Information provided by Daelim H&L

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 58.8 MPaASTM D1708
Elongation at Break 4.5 %ASTM D1708
Flexural Strength 76.5 MPaASTM D790
 39.2 MPa
@Temperature 260 °C
ASTM D790
Flexural Modulus 3.285 GPaASTM D790
 1.814 GPa
@Temperature 260 °C
ASTM D790
Compressive Strength 34.3 MPa
@Strain 1 %
ASTM D695
 127.5 MPa
@Strain 10 %
ASTM D695
Compressive Modulus 2452 MPaASTM D695
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
@Temperature 23.0 - 260 °C
ASTM D696
Maximum Service Temperature, Air 300 °CContinuous
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dielectric Polymers NT-583 Linered Polyimide Film Tape
DuPont™ Kapton® 100FPC Polyimide Film, 25 Micron Thickness
DuPont™ Kapton® 100HN Polyimide Film, 25 Micron Thickness
DuPont™ Kapton® 100KN Polyimide Film, 25 Micron Thickness
DuPont™ Kapton® 100VN Polyimide Film, 25 Micron Thickness

PDAEL911 / 178358

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.